Khyati Upadhyay, Abhay Dasadia, Sandip V. Bhatt, 等. Determination of optical properties of single crystal diamond substrates grown via welding-assisted microwave plasma enhanced chemical vapour deposition[J]. Functional Diamond, 2024,4(1).
Khyati Upadhyay, Abhay Dasadia, Sandip V. Bhatt, et al. Determination of optical properties of single crystal diamond substrates grown via welding-assisted microwave plasma enhanced chemical vapour deposition[J]. Functional Diamond2024, 4(1).
Khyati Upadhyay, Abhay Dasadia, Sandip V. Bhatt, 等. Determination of optical properties of single crystal diamond substrates grown via welding-assisted microwave plasma enhanced chemical vapour deposition[J]. Functional Diamond, 2024,4(1). DOI: 10.1080/26941112.2024.2350967.
Khyati Upadhyay, Abhay Dasadia, Sandip V. Bhatt, et al. Determination of optical properties of single crystal diamond substrates grown via welding-assisted microwave plasma enhanced chemical vapour deposition[J]. Functional Diamond2024, 4(1). DOI: 10.1080/26941112.2024.2350967.
Lab grown single crystal diamonds (SCDs) offer unrivalled hardness
a wide range of optical transparency
and supremely high thermal conductivity reliable materials to be a part of devices run at high frequency
temperature
and power. Effective synthesis techniques are essential in enhancing the potential applications of high-quality SCDs. This study aims to decrease the thermal contact resistance between diamond seeds and the molybdenum holder by utilizing welding material. Quality of grown diamond substrates (plates) were assessed by analysing optical properties through Raman
UV-Vis
and FT-IR spectroscopic methods. The findings revealed that the grown single-crystal diamonds have excellent transmittance (
>
70%) and absorption at 270 nm. Calculations also showed an average absorption coefficient of 1.1 cm
−1
indicating the high quality of the grown SCDs with nitrogen impurities below 10 ppm. The absorption observed in the FTIR spectra
ranging from 1600 cm
−1
to 2700 cm
−1
with a peak at 2354.13 cm
−1
is referred to as the “two phonon region
” which
is a distinctive feature of the diamond phase.
Field JE. The properties of diamond. London: Academic Press; 1979. (Open in a new window)Google Scholar
Thomas ME, Tropf WJ. Optical properties of diamond. Johns Hopkins APL Tech Dig. 1993;14:16–23. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Godfried, et al. U.S. Patent No. USO09551090B2. U.S. Patent and Trademark Office: Washington, D.C. 2017. https://patents.google.com/patent/US9551090B2/en(open in a new window). (Open in a new window)Google Scholar
Kitzler O, Sabella A, et al. Design and characterisation of optical quality single crystal diamond for raman laser applications. Proceedings of the International Quantum Electronics Conference and Conference on Lasers and Electro-Optics Pacific Rim 2011, (Optica Publishing Group, 2011). 2011. (Open in a new window)Google Scholar
Shreya N. Growth and characterization of large, high quality single crystal diamond substrates via microwave plasma assisted chemical vapor deposition [PhD thesis]. East Lansing, Michigan, US: Michigan State University; 2015. (Open in a new window)Google Scholar
Charris-Hernandez A. Towards the rapid growth of high quality, polycrystalline rimless and large area single crystal diamond substrates [PhD thesis]. East Lansing, Michigan, US: Michigan State University; 2017. (Open in a new window)Google Scholar
Yang B, Shen S, Zhang L, et al. Study on diamond temperature stability during long-duration growth via MPCVD under the influence of thermal contact resistance. J Appl Crystallogr. 2022;55(2):240–246. (Open in a new window)Google Scholar
European Carbon and Graphite Association. wegiel wzor [Photograph]. 1995. https://ecga.net/what-is-graphite/(open in a new window). (Open in a new window)Google Scholar
Cao GZ, Schermer JJ, van Enckevort WJP, et al. Growth of {100} textured diamond films by the addition of nitrogen. J Appl Phys. 1996;79(3):1357–1364. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Jin S, Moustakas TD. Effect of nitrogen on the growth of diamond films. Appl Phys Lett. 1994;65(4):403–405. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Müller-Sebert W, Wörner E, Fuchs F, et al. Nitrogen induced increase of growth rate in chemical vapor deposition of diamond. Appl Phys Lett. 1995;68(open in a new window)(6(open in a new window)):759–760. https://doi.org/10.1063/1.116733 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Afzal A, Rego CA, Ahmed W, et al. HFCVD diamond grown with added nitrogen: film characterization and gas-phase composition studies. Diamond Relat Mater. 1998;7(7):1033–1038. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Luo H, Ajmal KM, Liu W, et al. Polishing and planarization of single crystal diamonds: state-of-the-art and perspectives. Int J Extrem Manuf. 2021;3(open in a new window)(2(open in a new window)):022003. doi: 10.1088/2631-7990/abe915 (Open in a new window)Google Scholar
Upadhyay K. Enhancement in the quality of single crystal diamond seed substrate through various etching method. In: National Conference on Advances in Physical Science for Sustainable Development, August 27, 2022, Gandhinagar. Sector 15 Gandhinagar: A book on National Conference on Advances in Physical Science for Sustainable Development, pp. 114–124. 2023. (Open in a new window)Google Scholar
Altukhov AA, Vikharev AL, Gorbachev AM, et al. Characterization of single crystal diamond grown from the vapor phase on substrates of natural diamond. Semiconductors. 2011;45(open in a new window)(3(open in a new window)):392–396. doi: 10.1134/S106378261103002X (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Prawer S, Nemanich RJ. Raman spectroscopy of diamond and doped diamond. Philos Trans R Soc A. 2004;362(open in a new window)(1824(open in a new window)):2537–2565. https://doi.org/10.1098/rsta.2004.1451 (Open in a new window)Google Scholar
Ferrari AC, Robertson J. Interpretation of Raman spectra of disordered and amorphous carbon. Phys Rev B. 2000;61(open in a new window)(20(open in a new window)):14095–14107. http://dx.doi.org/10.1103/physrevb.61.14095 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Birrell J, Gerbi JE, Auciello O, et al. Interpretation of the Raman spectra of ultra nanocrystalline diamond. Diamond Relat Mater. 2005;14(open in a new window)(1(open in a new window)):86–92. doi: 10.1016/j.diamond.2004.07.012 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Wagner J, Wild C, Koidl P. Resonance effects in Raman scattering from polycrystalline diamond films. Appl Phys Lett. 1991;59(open in a new window)(7(open in a new window)):779–781. https://doi.org/10.1063/1.105340 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Bennett AM, Wickham BJ, Dhillon HK, et al. Development of high purity, optical grade single crystal CVD diamond for intra-cavity cooling. Proceedings of SPIE 8959, Solid State Lasers XXIII: Technology and Devices. 2014. http://dx.doi.org/10.1117/12.2037811 (Open in a new window)Google Scholar
Breeding CM, Shigley JE. The “type” classification system of diamonds and its importance in gemology. Gems Gemol. 2009;45(open in a new window)(2(open in a new window)):96–111. doi: 10.5741/GEMS.45.2.96 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Pandit T. Absorbance and Transmittance measurement of CsI thin films. In: Jain S, editor. Proceedings of the DAE Symposium on Nuclear Physics; Nabhikiya Urja Bhawan Auditorium, Anushakti Nagar, Mumbai-INDIA; 2013. p. 838–839. (Open in a new window)Google Scholar
Wang W, Hall MS, Moe KS, et al. Latest-generation CVD-GROWN synthetic diamonds from apollo diamond inc. Gems Gemmol. 2007;43(4):294–312. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Chrenko RM, Strong HM, Tuft RE. Dispersed paramagnetic nitrogen content of large laboratory diamonds. Philos Mag. 1971;23(182):313–318. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Sumiya H, Satoh S. High-pressure synthesis of high-purity diamond crystal. Diam Relat Mater. 1996;5(11):1359–1365. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Kiflawi I, Mainwood A, Kanda H, et al. Nitrogen interstitials in diamond, the American Physical Society. Phys Rev B. 1996;54(open in a new window)(23(open in a new window)):16719–16726. doi: 10.1103/PhysRevB.54.16719 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Litvak I, Cahana A, Anker Y, et al. Nitrogen structure determination in treated fancy diamonds via EPR spectroscopy. Crystals. 2022;12(open in a new window)(12(open in a new window)):1775. https://doi.org/10.3390/cryst12121775 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Hainschwang T, Notari F, Fritsch E, et al. Natural, untreated diamonds showing the A, B and C infrared absorptions (“ABC diamonds”), and the H2 absorption. Diam Relat Mater. 2006;15(10):1555–1564. (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Goss JP, Briddon PR, Hill V, et al. Identification of the structure of the 3107 Cm-1 H-related defect in diamond. J Phys. 2014;26(14):145801. (Open in a new window)Google Scholar
Petit T, Puskar L, Dolenko TA, et al. Unusual water hydrogen bond network around hydrogenated nanodiamonds. J Phys Chem C. 2017;121(open in a new window)(9(open in a new window)):5185–5194. doi: 10.1021/acs.jpcc.7b00721 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Stehlik S, Glatzel T, Pichot V, et al. Water interaction with hydrogenated and oxidized detonation nanodiamonds – microscopic and spectroscopic analyses. Diam Relat Mater. 2016;63(open in a new window):97–102. doi: 10.1016/j.diamond.2015.08.016 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Yang Z, Liang R, Zeng X, et al. A microscopy and FTIR and PL spectra study of polycrystalline diamonds from Mengyin kimberlite pipes. ISRN Spectroscopy. 2012;2012(open in a new window):1–10. doi: 10.5402/2012/871824 (Open in a new window)Google Scholar
Jiang T, Xu K. FTIR study of ultra dispersed diamond powder synthesized by explosive detonation. Carbon. 1995;33(open in a new window)(12(open in a new window)):1663–1671. doi: 10.1016/0008‐6223(95)00115‐1 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Jiang T, Xu K, Ji S. FTIR studies on the spectral changes of the surface functional groups of ultra dispersed diamond powder synthesized by explosive detonation after treatment in hydrogen, nitrogen, methane and air at different temperatures. Faraday Trans. 1996;92(open in a new window)(18(open in a new window)):3401. doi: 10.1039/ft9969203401 (Open in a new window)Google Scholar
Petit T, Puskar L. FTIR spectroscopy of nanodiamonds: methods and interpretation. Diamond Relat Mater. 2018;89(open in a new window):52–66. doi: 10.1016/j.diamond.2018.08.005 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Mitev D, Dimitrova R, Spassova M, et al. Surface peculiarities of detonation nanodiamonds in dependence of fabrication and purification methods. Diam Relat Mater. 2007;16(open in a new window)(4–7(open in a new window)):776–780. doi: 10.1016/j.diamond.2007.01.005 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Mironov E, Koretz A, Petrov E. Detonation synthesis ultra dispersed diamond structural properties investigation by infrared absorption. Diam Relat Mater. 2002;11(open in a new window)(3-6(open in a new window)):872–876. doi: 10.1016/S0925‐9635(01)00723‐3 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Krüger A, Liang Y, Jarre G, et al. Surface functionalisation of detonation diamond suitable for biological applications. J Mater Chem. 2006;16(open in a new window)(24(open in a new window)):2322–2328. doi: 10.1039/b601325b (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
Shenderova O, Petrov I, Walsh J, et al. Modification of detonation nanodiamonds by heat treatment in air. Diam Relat Mater. 2006;15(open in a new window)(11–12(open in a new window)):1799–1803. doi: 10.1016/j.diamond.2006.08.032 (Open in a new window)Web of Science ®(Open in a new window)Google Scholar
0
浏览量
1
Downloads
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621